Type MWd3 EKO/MWg3 EKO

PVC compounds MWd3 EKO and MWg3 EKO are used to generate inter alia: flat profiles, small building profiles, bathroom and furniture trunking. Mixtures are sold in dry blend powder or granulate.

Description


RequirementsUnitValue
Density g/cm3 1,57
Thermal stability at 200 0 C min 54
Vicat softtening temperature deg C 85
Hardness SHORE D 82
Elongation at break % 150
Max.tensile stress MPa 50


Packing


Mixtures are packed in polypropylene bags, type  big bags coated insidepolyethylene with capacity of 1 ton. Mixtures should be kept in rooms with temperature no higher than 35oC and humidity  not more than 75%, on wooden pallets.